Data Sheets » Test Results
Optical InterLinks (OIL) Polymer Products successfully completed outgassing tests. The testing was conducted by NuSil Technology LLC of Carpinterial, California. Outgas tests meeting ASTM E-595 were completed on typical material structure of OIL polymer film based products. Results indicate that Collected Volatile Condensable Material (CVCM) was less than the acceptable 0.10% maximum and Total Mass Loss (TML) is significantly below the accepted maximum of 1.00% after Water Vapor Recovered (WVR) is taken into account. Five grams of material were used in conducting the outgas testing. This mass was divided equally between one control sample and three testing samples. (Note: The testing mass is equivalent to more than 300 typical stand alone polymer devices.)
NuSil Report 
|
|
|
| |
|
|
|
|